How to store filament so it stays dry: dry boxes, vacuum bags and desiccant
By Sina Esfahani, OmniTechs · Published 27 November 2026
Keep every opened spool in an airtight container with dry desiccant and a hygrometer. UltiMaker advises below 20 % relative humidity for most filaments. Use a gasketed box for spools you print often, and a vacuum bag with fresh desiccant for spools you will not need for weeks. When the hygrometer starts to climb, regenerate the desiccant; CNC Kitchen does it as soon as the box reads above 10 %.
How strict you need to be depends on the material. Bambu Lab says PLA can be stored normally at 50 to 60 % humidity, while nylon, PVA, TPU and PETG absorb the most (Polymaker) and get the best boxes. Storage keeps dry filament dry. It is not a quick way to rescue a wet spool: dry that first.
Do it in this order:
Sort your spools: nylon, PVA, TPU and PETG first, PLA last (Polymaker, Prusa).
Dry any spool whose storage history you do not know before it goes into a box (Polymaker).
Choose the container: a gasketed box for spools in use, a vacuum bag with desiccant for long storage (UltiMaker, Prusa).
Add enough dry desiccant; a saturated pack can do more harm than good (CNC Kitchen).
Put a hygrometer inside; aim below 20 % and regenerate the desiccant above about 10 % (UltiMaker, CNC Kitchen).
Regenerate silica the maker's way, for example 80 to 90 °C and never above 100 °C for Bambu Lab's packs.
Keep the box cool, dark and away from temperature swings, and reseal each spool right after printing (UltiMaker, Bambu Lab).
Which storage suits which spool
Storage options compared
| Option | Best for | Watch out for |
|---|---|---|
| Open shelf | PLA you use within weeks, in a dry room (UltiMaker) | Not for nylon, PVA, TPU or PETG |
| Gasketed box with desiccant and hygrometer | Several spools in regular use | The desiccant must be regenerated; cardboard spools bring water in |
| Vacuum bag with desiccant | Spools you rarely use (UltiMaker) | The seal must hold; bags can develop holes, do not stack and hide the colour |
| Dry box you print from | Nylon, TPU or PVA during long prints | Keeps filament dry while printing; it is not a dryer (Polymaker) |
| Desiccant cabinet that regenerates itself | Many spools with little maintenance | Slowly dries PLA and PETG, but not enough for nylon (CNC Kitchen, in a test sponsored by one cabinet maker) |
How dry is dry enough
The makers do not publish one number, and their figures are far apart.
Storage humidity guidance by source
| Source | Humidity guidance | Other storage guidance |
|---|---|---|
| UltiMaker | Below 20 % for most filaments; its PVA below 50 % | Most of its filaments at −20 to +30 °C, ABS at 15 to 25 °C, PVA at 10 to 30 °C |
| Bambu Lab | PLA can be stored at 50 to 60 %; PETG absorbs moisture at 50 to 60 % | AMS level C or above means a relatively humid chamber |
| Prusa | No figure: a closed box with desiccant, or a vacuum bag with desiccant | Give the most hygroscopic materials priority |
| Polymaker | No figure: airtight bags, dry boxes with desiccant or vacuum containers | New spools ship vacuum-sealed with desiccant |
| CNC Kitchen | Regenerate the desiccant above 10 %; nylon kept absorbing even at about 15 % | A sealed box with plenty of silica |
A hygrometer reading also moves with temperature. Bambu Lab's example: 30 % relative humidity holds 4.7 g of water per cubic metre at about 20 °C, but 5.9 g at about 24 °C. Readings also rise after drying as the box cools. A reading that climbs overnight in a cold room is not always a leak.
Do not trust one cheap sensor. On the 3D Printing Stack Exchange, a dry box builder found one sensor reading about 16 % where four others read 6 to 9 %. CNC Kitchen notes that even professional loggers can be 5 percentage points off at these low levels, and that a cabinet's built-in hygrometer read too optimistically. Compare two sensors, and log the reading over days: an answer in the same thread treats a steady, straight-line rise as a small leak.
UltiMaker adds a shelf life: one year for PVA, nylon and TPU 95A under proper storage, up to two years for PP and PC. For the signs that a spool has already taken up moisture, see signs of wet filament.
Dry box: what makes one work
A dry box is any sealed container that holds spools and desiccant. Three things decide whether it works.
The seal. UltiMaker's DIY suggestion is a large plastic tote with weather stripping. Bambu Lab's check for its AMS units is the same idea: a seal strip that fits, and a lid that closes completely without deforming.
Enough dry desiccant. CNC Kitchen's tests show that to keep the air below 20 %, the desiccant must stay below roughly 10 % of its capacity. One cardboard spool can bring in more water than several small bags can hold.
Regular regeneration. A sealed box with desiccant is cheap, CNC Kitchen says, but only if you watch the hygrometer and regenerate on time.
Worked example from the same Stack Exchange thread: an IKEA Samla box with foam tape between lid and box reached about 1 % after fresh silica went in. It then rose in a straight line to 10 to 12 % over three months, which is when its owner dries the silica again. That gives you a rhythm to plan around.
A good box also slowly helps. CNC Kitchen put undried PLA and PETG in a sealed box with plenty of silica and they lost a significant amount of moisture in a week. Polymaker is more cautious: a box with desiccant is good for storage after drying, but less effective for active drying. If you print hygroscopic materials, you can print straight from a box; CNC Kitchen does, and Prusa sells dry boxes for it.
CNC Kitchen's early video shows a simple dry box built from a storage box and silica gel that you can print from.
Vacuum bags: good for long storage if the seal holds
Prusa and UltiMaker both suggest vacuum bags with a desiccant pack inside, and Polymaker ships its spools that way. In a popular thread on the Bambu Lab forum, the author explains why they work: less air in the bag means less water that the filament can take up. The seal is what matters; the desiccant only catches what is left.
Put the desiccant beside the filament, not in the hub. When the bag collapses against the spool, the hub becomes a separate pocket that the desiccant cannot reach (same thread).
Check the bag after a few days. A bag that is no longer tight has lost its seal; one user in the thread had bags develop holes.
Reuse the original bag. Put the spool back in the bag it came in, but dry or replace the desiccant pack first.
The trade-off is convenience: bags are fiddly to seal, do not stack and hide the colour, while big bins mean digging for the right spool (opening post of a second, long-running Bambu Lab forum thread).
Desiccant: which type, and how to keep it working
Desiccant types and the makers' notes
| Desiccant | What the sources say |
|---|---|
| Silica gel | Bambu Lab: its AMS beads change colour when spent (yellow to purple on its desiccant page). CNC Kitchen no longer recommends indicating desiccant for health reasons and uses a hygrometer instead |
| Molecular sieve | Bambu Lab: lowers humidity faster than silica at room temperature and keeps working at high drying temperatures |
| Calcium chloride | Bambu Lab no longer fits it in new AMS units: it can dissolve and leak, corroding electronics. A saturated pack looks like grease but is not; check it every two weeks and replace it within three months |
Silica can be regenerated, but follow the instructions for the product you have:
Bambu Lab's silica packs: oven at 80 to 90 °C, never above 100 °C, for 1 to 2 hours when light purple and 2 to 3 hours when dark purple. Reuse them 5 to 15 times. Use a dedicated tray, not one for food.
CNC Kitchen's bulk silica: 110 °C for 2 hours.
Polymaker's PolyBox bags: reusable 4 to 5 times, following the manual.
Store dried desiccant in a sealed bag until you need it (Bambu Lab). This CNC Kitchen video, linked at its chapter on the problem with desiccant, tests desiccant bags and ways to dry them.
Common mistakes
A random silica pack in the bag. A pack that is already saturated adds moisture instead of removing it (CNC Kitchen).
Trusting the box to dry a wet spool. Dry it first; storage only keeps it dry (Polymaker).
One cheap hygrometer. Compare it with a second one before you believe a low reading.
Cardboard spools in the dry box. In CNC Kitchen's test, a PLA on a cardboard spool lost more than 1 % of its weight, mostly water from the cardboard.
A cold spool into warm, humid air. Moisture can condense on it. That surface water evaporates quickly, unlike water absorbed into the core (CNC Kitchen).
When storage is not enough
Nylon and other technical materials. In CNC Kitchen's test, dried nylon kept absorbing moisture even at about 15 % in a desiccant cabinet. Dry it before each print, as Prusa also recommends for polyamide, PVA and BVOH.
A spool that snaps in the feed path. That is covered in brittle filament that snaps.
A leaking calcium chloride pack in an AMS. Switch the printer off and unplug it, then remove the pack and replace it with silica or molecular sieve; Bambu Lab warns that leakage can short-circuit the electronics.
Long storage in a heated dryer. CNC Kitchen warns that repeated heat cycles in a dryer's storage mode can slowly damage the polymer. See choosing a filament dryer and the filament drying chart.
Next step and related guides
Start with the spools that matter most: nylon, PVA, TPU and PETG in sealed boxes with dry desiccant and a hygrometer, PLA in a closed container or its original bag. Write the date you last regenerated the desiccant on the box. When a spool shows the signs of moisture anyway, dry it with the maker's cycle before printing.
Nylon has its own needs, explained in the nylon guide. If a spool keeps letting you down and you need the part more than the practice, the 3D printing service prints PLA and PETG parts from your file.