Wash and cure resin prints: the right times, and how to fix a tacky surface

By Sina Esfahani, OmniTechs · Published 27 November 2026

Every resin print leaves the printer coated in liquid resin. Washing removes that coating. Curing then finishes the hardening with light, and often heat, so the part reaches its full strength. Wash first and cure second, always: resin left on the surface is cured onto it (Anycubic).

For most hobby resins the times are short. Wash in IPA of at least 95% for 2 to 4 minutes, and no more than 10 minutes in total. Let the part dry completely, then cure it under 405 nm light: about 1 to 2 minutes for a miniature and 5 to 10 for a large model in a curing station. A tacky surface almost always means resin was left behind by dirty solvent. Wash it again in clean solvent, dry it, and cure again. Your resin maker's own times always win over these general figures.

Do it in this order:

  1. Gloves and glasses on, in a ventilated room with no flames nearby; let resin drip off the plate and drain it out of any hollow part.

  2. Rinse the print briefly in a first bath of used IPA, then wash it 2 to 4 minutes in clean IPA of 95% or more.

  3. Touch-test with gloves: still sticky and the solvent cloudy? Rewash at once in fresh solvent.

  4. Keep the total time in IPA under 10 minutes; longer can crack the print later.

  5. Wipe it, then let it dry completely: 5 to 10 minutes after wiping, up to 30 minutes in air. Never use a heat gun while alcohol is on it.

  6. Cure in a curing station: 1 to 2 minutes for a miniature, 3 to 5 for an average model, 5 to 10 for a large one, turning it so every side gets light.

  7. Replace the IPA once clean-looking parts stay tacky; on Formlabs' hydrometer that is about 10% resin.

Diagnose your print

What you see, what it means and what to do

Causes and fixes from the Formlabs, Anycubic, Elegoo and Prusa documentation, read 27 November 2026.
What you seeWhat it meansWhat to do
Sticky straight after washing, cloudy solventThe solvent is saturated with resinRewash at once in fresh solvent (Anycubic, Formlabs)
Still tacky after curingA film of resin stayed on after the wash, or the curing unit is not workingRewash, dry, cure again; check that every lamp lights (Formlabs)
A white, chalky film after curingSolvent or resin was still on the surface when it curedDry fully before curing next time (Elegoo, Anycubic, Prusa)
Waxy feel after washing in TPMTPM residue on certain resinsRinse in water; it fades after curing or within about a week (Formlabs)
Fine cracks hours or a day laterToo long in solventKeep total wash time under 10 minutes (Prusa)
A thin part warped in the curing stationThin, unsupported or unevenly litCure with supports on; place it flat on the turntable (Formlabs)
Brittle or yellowedCured far too long, or stored in sunlightFollow the resin maker's time; store out of the sun (Anycubic, Formlabs)
Resin weeping out of a hollow partLiquid trapped insideDrain holes and an inside flush; see the hollowing guide

How long to wash, and in what

The makers agree on strong IPA and short times. They differ on the exact minutes because their resins and wash machines differ.

Washing in IPA according to the makers

As published in each maker's documentation, read 27 November 2026. Your resin's bottle or data sheet may give its own time.
MakerIPA strengthWash timeLimit the maker names
Elegoo, beginner guide95% or higherAbout 2 to 3 minKeep cleaning until the surface is dry and not sticky
Anycubic, Wash and Cure Plus95% or higher2 to 4 minRewash in fresh solvent if sticky and cloudy
Prusa, CW1 and CW1SNot statedAdjustableNo more than 10 min in total; over-washed parts can crack, even after 24 hours
Formlabs, Form Wash settings90% or higher for most resinsPer resin: Standard V5 5 min, V4 10 min, Tough 2000 V2 15 minDurable at most 20 min; High Temp at most 6 min; PU Rigid never in IPA

Formlabs explains why a dirty bath leaves a sticky print. After washing, a thin layer of resin dissolved in IPA coats the part; the IPA evaporates, the resin does not. So the last liquid that touches the part must be clean. That is the reason for two baths: a first rinse in used solvent takes off the bulk, and a short wash in clean solvent leaves a clean surface. Formlabs recommends that pre-rinse, a squeeze bottle of fresh solvent for details, and an extra 5 minutes when the bath already holds a lot of resin.

Longer is not safer. Prusa warns of tiny cracks on parts washed too long, and Formlabs warns that thin walls absorb solvent and can deform after long immersion.

When to replace the solvent

IPA keeps dissolving resin until it stops cleaning. Replace it when:

  • The hydrometer says so. Formlabs replaces IPA at about 10% resin, or 10 to 12% on its IPA page, and TPM at 30 to 32%.

  • Clean-looking parts stay tacky. For some resins Formlabs saw tackiness from more than 5% resin in the IPA (Draft, Tough 2000 V1) and from more than 10% for Durable.

  • It has been about two months of frequent use. That is Prusa's rule of thumb.

  • The touch test fails. A washed part is still sticky and the solvent is cloudy (Anycubic).

You can stretch a bath by leaving it in a clear, closed container in sunlight until the dissolved resin cures and settles, then filtering it (Anycubic). Used solvent is hazardous waste and never goes down the drain; disposing of resin and IPA waste explains where it goes.

Alternatives to IPA, and water-washable resin

IPA is flammable, with a flash point of 12 °C (Formlabs), and evaporates fast. Wash in a well-ventilated room away from heat, flames and sparks, and keep the container closed when you are not using it (Formlabs). The alternatives each come with conditions.

  • TPM (tripropylene glycol monomethyl ether): Formlabs calls it a viable alternative that dissolves roughly three times as much resin as IPA. Rinse the parts in water afterwards; some resins feel waxy until they are dry or post-cured.

  • Formlabs Resin Washing Solution: flash point 93.5 °C, evaporates very slowly, and parts must be rinsed in water.

  • Prusament Resin Cleaner (DPM): much less flammable and less volatile than IPA, followed by a water rinse (Prusa).

  • Methylated spirits, turpentine and other household solvents: none of the makers here validates them. Formlabs warns that an unvalidated solvent may be hazardous or damage the parts; use only what your resin maker names.

Water-washable resin is washed in tap water (Anycubic, Elegoo), but it is still a sensitiser: Elegoo's version carries H317 and even H318, serious eye damage. The wash water now holds dissolved resin. Anycubic lets the water go down the drain once the resin in it has cured in sunlight and been filtered out; Elegoo's data sheet says the product must not reach the sewer. This guide follows the stricter rule.

Formlabs' short video compares IPA and TPM, with chapters on choosing a solvent, switching over, measuring saturation and safety.

How to know if IPA or TPM is better for your workflow | SLA (Formlabs Support)

Dry completely before you cure

Curing a wet part causes defects: solvent or resin left on the surface can turn white when it cures (Elegoo, Anycubic). Wipe the part with a lint-free cloth and let it air-dry for 5 to 10 minutes (Anycubic), or about half an hour in a cool place (Elegoo); compressed air speeds this up (Elegoo). A few drops of IPA do no harm, but IPA mixed with liquid resin leaves white stains (Prusa). Some Formlabs resins set their own minimum: at least 10 minutes for Tough 2000 V2 and 30 for Tough 1000.

Do not speed this up with heat while alcohol is still on the part. Anycubic warns that a heat gun or hair dryer on a print containing alcohol may cause a fire.

Supports: remove them before or after curing?

The makers lean towards curing first. Formlabs post-cures most parts with the supports on, to preserve their shape and prevent warping, and removes only supports that block light. Anycubic describes both routes for washing: supports off first saves solvent but is harder and can splash liquid resin; supports on softens them in the bath.

If you remove supports before curing, keep your gloves on: the part still carries liquid resin, and Formlabs warns that sharp tools slip on resin-coated surfaces.

How long to cure

Curing guidance from the makers

Curing guidance published by Anycubic, Elegoo and Formlabs, read 27 November 2026. Formlabs times apply to its own Form Cure units and resins.
MakerExampleCuring guidance
Anycubic, curing guideMiniature, average and large model in a curing station1 to 2 min, 3 to 5 min and 5 to 10 min
Anycubic, Wash and Cure PlusGeneral use2 min, longer for complex surfaces
Anycubic, curing guideSunlightHours: 2 to 3 h for a miniature, about 10 h for a large model
Elegoo, beginner guideAny model, 405 nm lampVaries with size and structure
Formlabs, Form CureStandard V5 resins5 min without heat; 15 min at 60 °C for better properties
Formlabs, Form CureGrey, Black, White V430 min at 60 °C; full post-cure 60 min
Formlabs, Form CureTough 200060 min at 70 °C

Light only cures what it reaches. Turn the part so the underside is lit too; Anycubic warns that uneven curing can crack or deform a model. Formlabs adds that dense supports block light, that a thin flat part is best laid flat on the turntable, and that thick parts need longer because heat takes time to penetrate. Light alone cures the surface; heat brings the full mechanical properties.

Sunlight works, but slowly, and Formlabs calls the result weather-dependent. Behind a window it is slower still. The accepted answer to a Stack Exchange question on exactly this notes that ordinary glass blocks most but not all of the UV, so whether it works depends on the wavelengths your resin reacts to; its data sheet tells you.

The Formlabs guide below walks through washing, support removal and curing on its own printers. The order of steps carries over to any resin printer; the settings do not.

Post-Processing Form 4 & Form 4L Prints | Washing, Support Removal & Curing Guide (Formlabs Support)

Can you over-cure a resin print?

Here the makers disagree.

What the makers say about curing too long

Statements from each maker's documentation, read 27 November 2026.
MakerPosition
Formlabs, Form Cure settingsOver-curing is acceptable unless stated otherwise for a resin; thick, bulky parts need longer
Prusa, CW1 and CW1SExtended exposure to UV light is not a problem
Anycubic, curing guidesToo long makes the material brittle, prone to cracking and yellow, especially clear and light colours
Formlabs, brittle-parts guidanceParts stored in direct sunlight can become more brittle and change colour

The safe reading: cure for the time your resin maker gives, add time for thick parts, and do not leave prints in the curing station or on a sunny windowsill for days in the hope of making them stronger.

Worked example: a miniature and a large bust

A 30 mm miniature on supports. Rinse it for 1 minute in the used bath, then 2 minutes in clean 95% IPA: 3 minutes in total, well under Prusa's 10. Wipe it and let it air-dry for 10 to 30 minutes. Cure for 1 to 2 minutes, turn it over and give the underside another minute (Anycubic). It should now feel dry and smooth, not tacky.

A 20 cm hollow bust. Drain the cavity through its holes before washing, because trapped resin uses up the wash liquid (Anycubic). Wash 4 minutes, let the solvent run out of the holes into the bath, and flush narrow channels with a syringe of clean solvent (Formlabs). Dry for the full 30 minutes, then cure for 5 to 10 minutes, turning it halfway. Its inside sees little light, which is why the wash, not the curing time, keeps it safe. Hollowing and draining resin prints covers where the holes go.

When to stop and start again

  • Still tacky after a rewash in clean solvent and a second cure: check the curing unit. Formlabs says a lamp bank that stays dark means a faulty unit; contact the maker.

  • Painted before curing and now sticky through the paint: scrap it. The accepted answer to a Stack Exchange question on this says paint blocks the light, so the resin may never cure; treat it as hazardous waste.

  • A cracked hollow part leaking resin: gloves on, cure the leaking resin and the part, and dispose of them as resin waste.

  • Your skin reacts: stop and read resin printer safety at home before you carry on.

If a print fails before it ever reaches the wash, start with resin print not sticking to the build plate. To judge whether a finished resin print is good enough for display, see assessing resin for small display details. OmniTechs does not print resin; if a filament part in PLA or PETG could do the same job, the comparison of FDM, SLA and SLS helps you decide.