Can PLA get wet? What water, hot water and the dishwasher do to PLA and PETG

By Sina Esfahani, OmniTechs · Published 27 November 2026

Yes, PLA can get wet. It does not dissolve: Bambu Lab lists its PLA as insoluble in water, and in two lab studies PLA came through a week in water with its weight, size and strength intact. Over months and years, water slowly breaks PLA down, a process called hydrolysis.

Heat is the real limit. PLA softens from about 55 to 60 °C, and dishwasher programmes run at about 40 to 70 °C, so keep PLA out of the dishwasher. PETG lasts longer, with heat deflection figures of 68 to 76 °C, but neither Prusa, Bambu Lab nor UltiMaker calls it dishwasher safe.

Whether a print holds water depends mostly on how you print it: enough walls, thin layers and dry filament.

For a print that meets water, in this order:

  1. Wash PLA by hand in lukewarm water and keep it away from anything hotter than about 55 °C.

  2. If it must go in the dishwasher, print it in PP, or test PETG on your coolest programme first.

  3. For watertight walls, print at least 4 perimeters in PLA or PETG, or 2 in PP (Prusa's test).

  4. Use 0.15 mm layers or lower on a 0.4 mm nozzle (Prusa).

  5. If you cannot add walls, raise the flow ratio by 0.02 to 0.05 (Bambu Lab) or to 105 to 110% (Prusa).

  6. Dry the filament first, because moisture leaves holes in the lines (Bambu Lab).

  7. Fill the print and leave it on a dry tissue for 48 hours before you rely on it, as Bambu Lab did.

Water, hot water or the dishwasher: what each material takes

What PLA, PETG and PP take, by situation

Prusa watertight test and Knowledge Base; heat deflection at 0.45 MPa from Prusa, Bambu Lab and UltiMaker; Heikkinen et al. (2018); UltiMaker PP datasheet; Formlabs; Formfutura; Bosch programme names. Read 27 November 2026.
SituationPLAPETGPP
Rain, splashes, cold waterYesYesYes
Standing water for weeks, such as a vaseYes, with enough walls; can swell and wick in some conditions (Prusa)Yes, with enough wallsYes; the best water barrier in thin walls (Prusa)
Permanent immersion for yearsDoubtful: water slowly hydrolyses PLANo maker figureUltiMaker advises against long-term immersion for its PP
Water hotter than about 55 °CNo: past its heat deflection of 55 to 59 °CHolds its shape below about 68 to 76 °CHolds its shape below 99 °C (UltiMaker)
Dishwasher, programmes of about 40 to 70 °CNo (Formlabs)Not recommended: Formlabs lists two PETG brands as not dishwasher safeFormfutura calls its Centaur PP dishwasher proof

What water does to PLA

PLA takes up very little water and does not soften in cold water:

  • It does not dissolve. Bambu Lab lists its PLA as insoluble. Prusa says PLA can swell and act as a wick for water in some conditions, but its own Prusament PLA test pieces and PLA flower pots did not leak over a long test.

  • It absorbs little. In humid air (25 °C, 55% relative humidity), Bambu Lab's PLA Basic takes up 0.43% water and its PETG Basic 0.32%. Those figures are for moisture from the air, not for soaking.

  • A week in water changes nothing measurable. All ten printed plastics in Heikkinen's study came through a week in water, and in Kaptan's 2025 study a PLA+ grade kept about 100% of its strength after seven days, and PETG more than 97%.

  • Years are another matter. Water can slowly hydrolyse PLA and soften nylon, Heikkinen and colleagues warn. UltiMaker does not recommend its PLA for long-term outdoor use. Prusa adds that PLA only breaks down in specialised composting facilities above 80 °C and will not disintegrate in a garden compost heap, so a planter will not rot away.

Nylon is the material to watch. UltiMaker says water can damage it, and Prusa says badly stored nylon absorbs up to 10% of its weight in water.

Moisture in the spool before printing is a different problem: damp filament pops, strings and prints weaker parts, as the guide to signs of wet filament explains. For acids, alcohol and other liquids, see the chemical-resistance comparison.

Can PLA or PETG go in the dishwasher?

Water is not what damages a print in a dishwasher; heat is. Formlabs warns that most printing materials have a low heat deflection temperature, the point where a part bends under a light load, so parts can deform, warp or crack when hot. It says dishwashers rule out PET, nylon and PLA, because they soften and distort around 60 to 70 °C. Polymaker adds that a print can look fine at room temperature and still deform, leach or degrade after dishwasher cycles, hot water or detergents.

Heat limits of PLA and PETG in the makers' own figures

Heat deflection at 0.45 MPa (ISO 75) from Prusa's material table and Knowledge Base, Bambu Lab PLA Basic and PETG Basic datasheets V2.0, and UltiMaker PLA and PETG datasheets. Read 27 November 2026.
MaterialPrusaBambu LabUltiMaker
PLAHeat deflection 55 °C; soft and deforms above 60 °CHeat deflection 57 °CHeat deflection 58.8 °C; not for parts above 59 °C
PETGHeat deflection 68 °C; for use below 80 °CHeat deflection 69 °CHeat deflection 76.2 °C; not for parts above 76 °C

Now compare those figures with a dishwasher. Bosch names its programmes after their temperature: Glass 40°, Eco 50°, Auto 45° to 65°, Express 60° and Intensive 70°, and its Hygiene option keeps the final rinse at up to 70 °C. Your own machine's manual lists its programmes.

A worked example: PLA's heat deflection is 55 to 59 °C. Auto at up to 65 °C and Intensive at 70 °C both pass it, and even Eco 50° leaves only 5 to 9 °C of margin. PETG at 68 to 76 °C clears Eco and Auto on paper, but Intensive and a hygiene rinse at 70 °C sit above Prusa's and Bambu Lab's 68 and 69 °C. That is why:

  • PLA: wash it by hand in lukewarm water.

  • PETG: if you try it at all, use the coolest programme and put a spare print through it first. The table on the same Formlabs page lists two PETG brands as not dishwasher safe.

  • PP: Formfutura describes its Centaur PP as dishwasher proof, and UltiMaker sets its PP's limit at 99 °C. The polypropylene guide covers what printing it involves.

After a test run, check the spare print for warping, cracks and loose layers. The result holds for that material, design and programme only. Anything that touches food has its own rules, set out in the food-contact guide. For heat in general, including cars, see the heat-resistance guide.

Make a print hold water

Prusa found that leaks come mainly from the seams and from the joins between perimeters and solid infill, not from the bond between layers. The fix is a dense wall.

Settings for watertight prints from Prusa and Bambu Lab

Prusa blog, Watertight 3D printing part 1 (23 April 2021), and Bambu Lab Wiki, Guide to reduce the risk of prints leakage. Read 27 November 2026.
SettingPrusaBambu Lab
WallsAt least 4 perimeters for PLA and PETG; 2 for PP, ABS, ASA, PC and CPE2 to 4 wall loops
Layer height0.15 mm or lower on a 0.4 mm nozzle; thicker layers leaked moreLower layer height, wider lines
Flow105 to 110% if you cannot add perimeters, at the cost of accuracy and stringingRaise the flow ratio by 0.02 to 0.05
Temperature5 to 10 °C hotterNot given
BottomPerimeters matter more; 5 or more bottom layers to be safeConcentric bottom surface pattern
InfillNot needed at 100% if the walls are thick0 to 40%
Vase modeOne perimeter was watertight in every material testedNot given
FilamentNot givenDry it first, to avoid holes in the lines

Where to set them:

  • PrusaSlicer: perimeters under Print Settings, Layers and perimeters; flow under Filament Settings, Extrusion multiplier; the overlap between infill and perimeters under Print Settings, Advanced.

  • Bambu Studio: wall loops under Process, Strength; layer height under Process, Quality; the bottom surface pattern under Process, Strength; the flow ratio in the filament settings.

A worked example with the makers' own numbers. Prusa counts 2 to 4 perimeters as a thin wall of 0.9 to 1.8 mm, and found that from about 6 perimeters, a wall of 2 to 3 mm, the material no longer matters. So a PLA vase on a 0.4 mm nozzle needs at least 4 perimeters, about 1.8 mm. For flow, Bambu Lab's own example raises PLA Basic from 0.98 to 1.00 to 1.03.

Taboretum's video walks through watertight settings in PrusaSlicer and then in Bambu Studio, with most attention on vase mode, and ends by filling a printed cone with water. It starts at the Bambu Studio chapter.

Slicer Settings for WATERTIGHT Prints, Bambu Studio and Prusa Slicer (Taboretum)

Test with the liquid and the time the part will see. Bambu Lab left dyed water in its test vases for 48 hours on a dry tissue. For a part under pressure, an answer on the 3D Printing Stack Exchange suggests soaking a printed irrigation fitting for a month or two at its working temperature, then testing it under pressure again. Bambu Lab adds that settings lower the risk of leaks but cannot guarantee every model is leak-proof. For a vase, a separate tested insert is often simpler, as the guide to vases and watertight inserts explains.

Sealing a print that still leaks

Prusa lists four ways to seal a print after printing:

  • Clear acrylic lacquer, sprayed inside and out a few times, following the safety instructions on the can. It is the simplest, but Prusa does not recommend it for anything that touches food.

  • Nail polish, for small areas.

  • Epoxy resin. Messy and gives off fumes, so Prusa advises gloves and respiratory protection at a minimum; curing can take several days. For food, Prusa points to certified food-grade epoxy.

  • Chemical smoothing, which works with common, relatively safe solvents only for ABS, ASA, HIPS and PVB. The vapour-smoothing guide covers it and its safety.

Under pressure and outdoors

A box that must stay dry under water is harder than a vase. In its second watertight article, Prusa suggests walls of 2 to 3 mm, and for parts under pressure it starts testing at four perimeters and 60% infill. Above about 2 bar, it expects you to need post-processing such as epoxy. Prusa found the material less important than the settings: Prusament PLA worked at 20 m depth without treatment, while untreated PETG leaked quickly through its seams.

In this video Prusa shows how it built and tested a printed watertight light for underwater photography, with the trials and errors along the way.

Does 3D printing work at 40 m depth underwater? (Prusa 3D)

For prints that stand outside, UV light and heat matter as well as rain. The outdoor filament guide compares what makers publish on UV and weather.

If the part must survive the dishwasher, the polypropylene guide shows how to print PP. If it is a vase, the guide to vases and watertight inserts helps you choose between a printed and a separate insert. If it touches food, read the food-contact guide first.

If PETG suits your part and you need it printed rather than the practice, the PETG printing page explains what OmniTechs can print from your file.