Blobs and zits on 3D prints? Where they sit tells you the fix

By Sina Esfahani, OmniTechs · Published 27 November 2026

Zits are small bumps where the nozzle starts and stops a wall. Molten plastic does not stop or restart instantly, so every stop and start leaves a little extra material (Simplify3D). Blobs are the same thing, larger, or plastic that collected on the nozzle and dropped onto the part.

Where the bumps sit tells you the cause. Scattered all over usually means the seam is set to Random. One vertical line is the seam itself. Bumps at corners are pressure in the nozzle. Pits with a popping sound are wet filament. Brown blobs are build-up on the nozzle. Fix the cause the pattern points to, one setting at a time, on the same test part.

Fix it in this order:

  1. Bumps scattered over every wall: change the seam from Random to Aligned, Back or Nearest (Bambu Lab, Prusa).

  2. Popping, pits or craters: dry the filament; retraction settings alone usually cannot fix damp filament (Bambu Lab).

  3. Calibrate flow and pressure advance before you tune the seam gap, wipe or coasting.

  4. Bump at the start of each wall: prime less after a retraction and turn on wipe before the external loop (Simplify3D, OrcaSlicer).

  5. Bump at the end of each wall: widen the seam gap a little (Bambu Studio default 15% of the nozzle width) or try 0.2 to 0.5 mm of coasting (Simplify3D).

  6. Bumps where the nozzle lands after a travel: turn on avoid crossing walls and wipe while retracting, and keep retraction at 2 mm or less on direct drive (Bambu Lab, Prusa).

  7. Brown blobs with PETG: clean the nozzle, dry the spool and keep the flow ratio at 0.93 to 0.96 (Bambu Lab).

Read the pattern of the bumps

What the pattern of the bumps points to

Summary of the Bambu Lab, Prusa, OrcaSlicer, Simplify3D and Klipper pages and the Stack Exchange answers under Sources, read on 27 November 2026.
What you seeWhat it meansWhat to do
Bumps scattered over the whole surfaceSeam position set to RandomAligned, Back or Nearest, or paint the seam
Bumps in one vertical lineThe seam: the start and end of each wall loopSeam placement, seam gap, wipe, scarf seam
Bumps at the cornersPressure in the nozzle as the head slowsPressure advance or linear advance
A lump where printing resumes after a travel moveOoze during the travel, then re-primingAvoid crossing walls, wipe, retraction
Pits, craters or bubbles, with crackling or poppingMoisture in the filament turning to steamDry the filament
Larger brown or burnt blobs that get worse over a print, often PETGBuild-up on the nozzle falling offClean the nozzle, dry, lower flow or temperature
Rough, rippled surface everywhereToo much plastic, or the nozzle too closeFlow and first-layer height

Seam bumps: is it the start or the end of the wall?

Watch an outer wall being printed (Simplify3D's tip). If the bump appears the moment the nozzle starts the loop, the printer pushed out more plastic than it pulled back, or plastic oozed during the travel there. If it appears as the nozzle finishes the loop, pressure left in the nozzle is still pushing plastic out as it slows.

A bump at the start

The start is hard to get right because the nozzle arrives after a travel move, often after a retraction. OrcaSlicer's seam guide puts it this way: the less opportunity for ooze, the cleaner the start. Its list:

  • Calibrate pressure advance. Too low leaves pressure in the nozzle at the end of the last line, which oozes during the travel.

  • Make travel moves as fast as your printer allows, so there is less time to ooze.

  • Turn on Wipe before external loop (Process, Quality, Seam), so the restart happens inside the part.

  • Raise the Travel distance threshold to 2 to 4 mm, so tiny moves do not trigger a retraction and restart at all.

  • Turn on retract on layer change, so every layer starts the same way.

  • Print the walls inner, outer, inner, or else inner then outer (Walls printing order). Starting the outer wall straight after a long travel leaves the most visible marks.

If it still primes too much, prime less. Example from Simplify3D: with a retraction of 1.0 mm and an extra restart distance of -0.2 mm, the extruder pulls back 1.0 mm but pushes only 0.8 mm forward again. In Cura, check that Retraction Extra Prime Amount (Travel) is still 0; it adds material after a retraction.

A bump at the end

The end is easier: the nozzle only has to stop extruding at the right moment. Tune pressure advance first; OrcaSlicer says too low a value leaves a wider line where the loop ends, and too high a value leaves a gap. Then use the seam gap, which stops the loop slightly early to leave room for the excess. Bambu Studio's default is 15% of the nozzle diameter, which is 0.06 mm on a 0.4 mm nozzle; OrcaSlicer calls 0 to 15% typical for a well-tuned printer and suggests a slightly larger gap if the seam bulges. PrusaSlicer has the same idea as Seam gap distance.

Coasting does a similar job by switching off extrusion just before the end of the loop. Simplify3D says 0.2 to 0.5 mm of coasting is typically enough to make a noticeable difference. Cura calls it Enable Coasting (Experimental) and sets it as a volume, by default 0.064 mm³.

Hardware matters too. OrcaSlicer's guide reports that high-flow nozzles with a large melt zone make worse seams than standard ones, and a 0.6 mm nozzle worse than a 0.4 mm one. The retraction guide explains distance, speed and wipe for Bowden and direct-drive printers.

Random seams scatter zits; aligned seams line them up

Every wall loop has to start somewhere. Bambu Lab calls a Random seam position the most common reason for dots scattered over the walls, and Prusa describes Random as making the seam less noticeable "at the cost of a less smooth surface". Random makes little sense on a model with corners, where Nearest or Aligned can tuck the seam into one; it can work on a cylinder (Prusa).

Where to change it:

  • Bambu Studio and OrcaSlicer: Process, Quality, Seam, Seam position.

  • PrusaSlicer: Print Settings, Layers and perimeters, Seam position.

  • UltiMaker Cura: Walls, Z Seam Alignment.

So choose the trade-off deliberately: one line you place at the back or in a corner, or bumps spread thinly over the whole part. Scarf seams overlap the start and end of a loop in a gentle ramp to hide it on smooth, curved walls; they arrived in Bambu Studio 1.9, and PrusaSlicer has them as scarf joint placement. Prusa notes they add print time and help less in sharp corners and on overhangs. The seam cannot be eliminated except in vase mode, with one wall and no infill (Prusa). Placement, painting and scarf settings are covered in hide the Z seam.

Bambu Lab's own video walks through seam position, alignment and scarf seams in Bambu Studio.

Bambu Studio Seam Control - Hide Seam Lines in your 3D Prints (Bambu Lab Support)

Bumps at corners: pressure in the nozzle

Molten plastic under pressure does not respond instantly when the head slows for a corner, so it bulges there. Pressure advance (linear advance in Marlin) does two things, according to Klipper: it reduces ooze during non-printing moves and it reduces blobbing at corners. On Klipper's tuning tower, layers below the right value show blobs at the corners, and layers above it rounded corners. Prusa names linear advance and the extrusion multiplier as the settings that most affect how visible the seam is. The full procedure is in pressure advance and linear advance.

In this video Minimal 3DP shows how corner bulges and gaps look, then runs OrcaSlicer's three pressure advance tests (tower, line and pattern) and reads the results.

Blobs on Every Corner? Fix It With OrcaSlicer Pressure Advance (Minimal 3DP)

Ooze during travel moves

When the nozzle moves without printing, heat and pressure keep plastic seeping out. It lands as a lump where printing resumes. Bambu Lab lists the usual causes: long travel moves with too little retraction, models with many separate islands or parts spread far apart on the plate, a nozzle that is too hot, and damp filament.

Keep the travel inside the part, where ooze stays hidden:

  • Bambu Studio and OrcaSlicer: Avoid crossing walls; Wipe while retracting under the printer's Extruder settings. Bambu Lab says the wipe reduces blobs when printing restarts after a travel.

  • PrusaSlicer: Avoid crossing perimeters (Print Settings, Layers and perimeters, Quality) and Only retract when crossing perimeters (Print Settings, Infill, Advanced). Prusa recommends leaving Wipe while retracting on (Printer Settings, Extruder 1).

  • UltiMaker Cura: Combing Mode and Avoid Printed Parts When Traveling (Travel), both on by default, and Outer Wall Wipe Distance (Walls, 0.2 mm by default).

More retraction is not always better. Bambu Lab generally recommends no more than 2 mm on its printers, because too much causes under-extrusion, gaps and clogs. Prusa gives a maximum of 2 mm for its MK2.5 and MK3 series and uses 3.2 mm on the Bowden-fed MINI. If you suspect the nozzle temperature, Prusa suggests testing 5 to 10 °C lower.

Pits, popping or brown blobs: dry the filament, clean the nozzle

Wet filament

Moisture in the filament turns to steam in the hot nozzle. Bambu Lab names it the second common cause of dots on walls: the water boils away as the plastic leaves the nozzle and leaves small gaps and imperfections. It recommends drying every spool before printing, new ones included. Answers on the Stack Exchange question about bubbles in extruded filament, viewed more than 57,000 times, point to moisture, which you can often hear as crackling, and to printing too hot. See signs of wet filament and the filament drying chart for the makers' temperatures.

Build-up on the nozzle

Some blobs are not seams at all but plastic that collected on the outside of the nozzle and fell onto the part, often brown or burnt. Bambu Lab says this happens mostly with PETG-type filaments and lists five causes:

  1. Damp filament, one of the most common causes. Steam pushes the melt outwards until it touches and sticks to the nozzle. Dry the spool and store it below 20% relative humidity.

  2. Flow ratio too high. For PETG-type filament Bambu Lab gives 0.93 to 0.96; its own PETG Basic and PETG-CF default to 0.95. If the filament is dry, check the nozzle for wear and replace a worn one; if it is not worn, try 0.93 to 0.94.

  3. Speed and temperature that do not match. If you slow the print by lowering the maximum volumetric speed by 4 to 5 mm³/s, lower the nozzle temperature by 5 to 10 °C as well.

  4. A worn or loose nozzle wiper, on printers that have one. It leaves residue on the nozzle; repair or replace it.

  5. Many travel moves. Ooze collects on the nozzle during each one; lay the parts out so long travels are few.

Heat the nozzle first, then remove the build-up carefully (Bambu Lab). Prusa adds that long PETG prints leave a thin layer on the nozzle, so clean it thoroughly before printing. For PETG settings see PETG print settings; for strings rather than bumps, diagnose PETG stringing.

Too much plastic makes every bump bigger

If the whole surface is rough and rippled, the printer may simply be laying down more plastic than fits. The top answer on a Stack Exchange question about rough surfaces, with more than 57,000 views, traces it to over-extrusion or a nozzle set too close to the bed. Prusa likewise suggests a slightly lower extrusion multiplier to make the seam less visible. Calibrate flow with the flow rate calibration guide and check the first-layer height with setting the z-offset before you tune seams.

When to stop tuning

Accept a faint, tidy seam line: Prusa says FDM cannot eliminate the seam, only make it less noticeable. If you need a wall with no seam at all, vase mode is the only route.

Stop tuning settings and look at the hardware when blobs keep coming back with dry filament and calibrated flow. A worn nozzle causes build-up (Bambu Lab). Burnt plastic packed around the nozzle after a nozzle change can mean the hotend leaks between the heater block and the heat break, as one asker on Stack Exchange suspected on a Prusa MK3S; reassemble the hotend to the maker's instructions before printing again.

Start with the seam: hide the Z seam shows how to place, paint and scarf it once the bumps are under control. If the corners still bulge, tune pressure advance. And if you print PETG, its stringing and nozzle build-up share causes; diagnose PETG stringing tests them one by one.