Bed temperature for PLA and PETG: the right setting for your build plate
By Sina Esfahani, OmniTechs · Published 27 November 2026
On a PEI sheet, start PLA at 55 to 60 °C and PETG at 70 to 80 °C. For PLA, that sits inside what Bambu Lab's plate guide, Prusa, Prusament and Polymaker publish, and Bambu Lab's own PLA default on textured PEI is 55 °C. For PETG, 70 to 80 °C is where the ranges of Bambu Lab, Prusament and Polymaker's PolyLite PETG overlap; Prusa runs its own sheets hotter. Coated low-temperature plates need less: Bambu Lab's Cool Plate SuperTack holds PLA from 40 °C and PETG at 55 to 60 °C.
The filament maker's value for your plate comes first; adjust from there in steps of 5 °C. Too cold and corners lift. Too hot and you get elephant's foot, soft lower layers, prints that will not let go and, in an enclosed printer, filament softening in the extruder. Keep the bed on for the whole print.
Set it in this order:
Select the plate type in the slicer that is actually on the printer.
Use the filament maker's value for that plate; without one, PLA at 60 °C and PETG at 75 °C on PEI.
Corners lift: raise the bed by 5 °C, then 5 °C more if needed (Bambu Lab).
The bottom flares or prints stick too hard: lower it in 5 °C steps.
Room below 20 °C or an open-frame printer: add about 10 °C (Bambu Lab).
PLA in an enclosed printer with the bed above 45 °C: open the door or lid (Bambu Lab).
Leave the bed on until the print has finished.
Published values per plate
Published bed temperatures for PLA and PETG per build plate
| Source | Plate | PLA | PETG |
|---|---|---|---|
| Bambu Lab filament guide | Textured PEI Plate | 45 to 65 °C; 55 °C is the default in its PLA guide | 60 to 80 °C |
| Bambu Lab filament guide | Smooth PEI or High Temperature Plate | 45 to 65 °C | 60 to 80 °C, with glue |
| Bambu Lab filament guide | Engineering Plate | 45 to 65 °C, glue required | 60 to 80 °C, with glue |
| Bambu Lab plate guide | Cool Plate SuperTack | Holds firmly from 40 °C | 55 to 60 °C on the second generation; about 65 °C on printers that share presets for both generations |
| Bambu Lab filament guide | Cool Plate or PLA Plate (discontinued) | 35 to 45 °C | Not recommended |
| Bambu PLA Basic datasheet V2.0 | Cool Plate, High Temperature Plate or Textured PEI Plate | 35 to 45 °C | Not on this sheet |
| Prusa Knowledge Base | Prusa PEI sheets: satin or smooth for PLA, textured or satin for PETG | 60 °C | 85 °C first layer, 90 °C after |
| Prusament product pages | Not tied to a plate | 40 to 60 °C, heated bed optional | 80 ± 10 °C, heated bed recommended |
| Polymaker wiki | PC and textured PEI, glue when needed | PolyLite PLA: 25 to 60 °C | PolyLite PETG: 70 to 80 °C; Polymaker PETG: 60 to 70 °C |
Two disagreements matter. Bambu Lab's PLA Basic datasheet gives 35 to 45 °C on all three plate types, while its filament guide gives 45 to 65 °C on the PEI plates and its warping guide aims for 55 to 65 °C on textured PEI. When a maker's datasheet and its plate guide differ, start from the plate guide and the slicer profile, which are written for the plate. And Prusa runs PETG at 85 to 90 °C, hotter than Bambu Lab's 60 to 80 °C. The bed values from 17 filament datasheets side by side are in PLA, PETG, ASA and TPU datasheets compared.
Why the plate type changes the number
The same material is usually printed at different bed temperatures on different plates (Bambu Lab). Most surfaces, PEI among them, grip better when hot, while mechanical surfaces such as painter's tape gain little from heat. A low-temperature coating such as SuperTack is designed to hold PLA and PETG with very little heat.
That is why the plate setting in the slicer matters. Select the wrong plate and the bed runs at the other plate's temperature; on Bambu Lab's textured PEI the printer also drops the extra 0.04 mm squish it applies for that surface. Where you set it:
Bambu Studio: the bed temperature lives in the filament preset, with a value per plate type.
OrcaSlicer: the filament settings, under Bed, with a first-layer and an other-layers value for each plate type.
PrusaSlicer: Filament Settings, Filament, Temperature.
Cura: Material, Build Plate Temperature and Build Plate Temperature Initial Layer.
Which plate suits which filament is covered in build plates compared.
Why the bed stays heated after the first layer
There are three reasons, set out in the accepted answer to the 3D Printing Stack Exchange question on exactly this point:
The bed expands when hot and contracts when it cools, so switching it off can make the part lose its grip and pop off mid-print.
The bed was levelled hot, and its shape changes as it cools.
The print needs warmth below it. The heated bed keeps the bottom few millimetres warm enough not to contract and lift the corners. A centimetre up, the print is already close to room temperature, which is why large prints in warping materials need a warm chamber as well.
Changing the value after the first layer is normal; switching the bed off is not. A drop of about 5 °C after the first layer is usually no problem, while larger drops or switching the heat off make parts come loose (3D Printing Stack Exchange). Prusa even goes up for PETG, from 85 °C on the first layer to 90 °C after it. If your bed switches itself off after a few layers, look for an energy-saving mode: on a Creality CR-10S Pro it is the Economic option in the Adjust menu (3D Printing Stack Exchange).
Do you need a heated bed for PLA?
Not for the material itself. Prusa says PLA does not require a heated bed, Prusament lists it as optional and Polymaker's PolyLite PLA range starts at 25 °C. Forum answers split the same way: one prints PLA at 40 °C on painter's tape, another prefers 60 °C. The surface decides. A PEI or SuperTack plate still needs the range its maker publishes, because that is how it holds the first layer.
Too hot or too cold: what each looks like
Reading the bed temperature from the print
| What you see | What it means | What to do |
|---|---|---|
| Corners lift or the part comes loose | Bed too cold for the plate, or a cold room | Raise 5 to 10 °C; add about 10 °C below 20 °C room temperature (Bambu Lab) |
| The bottom layer flares out | A hot bed keeps the first layer soft | Lower towards the bottom of the range, then use elephant foot compensation |
| PLA layers near the bed sag, gaps fuse, supports bond to the part | The bed is above the point where PLA softens, so the fan cannot set those layers | Lower the bed; Prusa says PLA softens above 60 °C, and Bambu Lab gives a heat deflection temperature of 57 °C |
| The print will not come off the cold plate | More heat means more grip (Bambu Lab) | Lower the bed next time |
| Clogs or thin extrusion with PLA in an enclosed printer | The warm chamber softens filament in the extruder | Open the door or lid once the bed is above 45 °C for PLA, or above 60 °C for PETG (Bambu Lab) |
Each symptom has its own guide: stop 3D prints warping, elephant's foot, print stuck to the bed and heat creep.
Example: the same PLA in summer and in winter
Bambu Lab's PLA default on textured PEI is 55 °C. In a hot summer room, its PLA guide opens the printer door and lowers the bed by 5 to 10 °C, to 45 to 50 °C, still inside the 45 to 65 °C range for that plate. In a garage below 20 °C it goes the other way: about 10 °C more, to 65 °C, the top of that range. Plate, filament and printer stay the same; only the room changed.
The number on the screen is not the plate surface
The display shows what the bed's sensor reads, and the surface you print on can be cooler. Many people set the bed well above the real surface temperature, and the right value is the one your prints confirm. Depending on how the heater is built, the gap can be anything from almost nothing to 20 °C or more (3D Printing Stack Exchange). Treat every published value as a starting point.
Thomas Sanladerer tested which heated bed setups heat evenly, which cope with cooling fans and how much they warp while heating up.
A bed that swings around its set point causes trouble of its own. CNC Kitchen found that a swing of only about 1 °C either way, under simple on-off (bang-bang) control, made the bed expand and deform enough to print thicker and thinner layers; switching back to PID control removed the marks. A variation of a few tenths of a degree is fine. Such marks look like Z banding. The link starts at the chapter on thermal bed deformation.
When to stop adjusting
A bed that cannot reach or hold its set temperature is a hardware problem, not a setting. If the printer shows a bed thermal runaway error, it has shut the heater down to protect you. Prusa notes that this can happen at high bed temperatures in rooms below about 18 °C. Warm the room or use an enclosure, never bypass the safety check, and switch the printer off and unplug it before you work on the bed or its wiring.
Next step and related guides
If the right temperature still does not hold the first layer, work through first layer not sticking. If you want a plate that needs less heat, build plates compared explains the coated options.
Sources
Prusa Knowledge Base: Extrusion stopped mid-print (heat creep)
3D Printing Stack Exchange: Why keep the bed heated after initial layer(s) with PLA (or PETG)?
3D Printing Stack Exchange: Heated bed, what are the benefits? Why use one?
3D Printing Stack Exchange: Consequences of setting the bed temperature too high with PLA?
3D Printing Stack Exchange: Altering the print bed temperature at different layers
3D Printing Stack Exchange: CR-10S Pro heated bed turns off after first few layers