3D print warping: stop the corners lifting, step by step
By Sina Esfahani, OmniTechs · Published 27 November 2026
Warping is shrinkage. Plastic contracts as it cools, and because the first layer is held by the plate, every layer above pulls the edges inwards and upwards. Big flat parts, sharp corners, dense infill, cold or draughty rooms and high-shrink materials warp most. Bambu Lab ranks the risk from PC, PA-CF, PA, ABS and ASA down to PETG and PLA.
The fix is to hold the base down and let it cool slowly. Get the grip right first: a clean plate, the right plate type and the right bed temperature. Then keep the bottom warm: no fan on the first layers, no draughts, and an enclosure for ABS, ASA, PC and nylon. Add a brim or brim ears where corners lift. If that is not enough, change the design or the material.
Fix it in this order:
Wash the plate with dish soap and warm water, then keep your fingers off it (Bambu Lab).
Check that the plate type in the slicer matches the plate on the printer.
Raise the bed by 5 to 10 °C; for PLA on textured PEI, Bambu Lab aims for 55 to 65 °C.
Switch the part fan off for the first 3 layers.
Block draughts, and print ABS, ASA, PC and nylon enclosed; Bambu Lab wants 40 °C or more in the chamber for ABS and ASA.
Add a brim of 8 to 10 mm, or brim ears on the corners that lift.
Still lifting: round the corners, use gyroid infill at 25% or less, or switch material.
Warping or something else?
What lifting corners can mean
| What you see | What it means | What to do |
|---|---|---|
| Corners curl up part-way through, sometimes with a ripple where the nozzle hit the lifted edge | Warping: the print shrinks as it cools | Follow the fix order above |
| The whole print shifts, slides or pops off | Adhesion failure: grease, the wrong plate type or a nozzle set too high | Re-run bed levelling, check the z-offset and the plate type |
| One corner never sticks, whatever you print | The bed sits lower in that corner | Level the bed |
| Uneven side walls or top layers while the corners look flat | Slight warping, easy to mistake for a flow problem | Treat it as warping before you change flow |
| Small parts or steep overhangs curl in an enclosed ABS or PC print | Too little cooling in that spot | Try the part fan at 10 to 20% (Prusa) |
A print that comes off whole is diagnosed in first layer not sticking; a corner that never sticks is a job for bed levelling.
Why prints warp, and which materials warp most
Hot, expanded plastic is laid on layers that have already cooled and shrunk. As it cools, it pulls the top of the layer below inwards, and that layer curls. The first layer cannot shrink because it is fixed to the plate, so the stress builds at the bottom, and the bigger the part, the harder its corners are pulled. That is how the accepted answer to a Stack Exchange question on warped print bottoms explains it. Less warping also means less residual stress, and a stronger part (Prusa).
CNC Kitchen shows the mechanism in a simple experiment of about a minute and a half.
Warping by material, as the makers describe it
| Material | What the makers publish | Enclosure |
|---|---|---|
| PLA | Prusament: warping susceptibility none; Prusa: not prone to significant warping | Not needed; Prusa says it makes the cooling PLA needs harder |
| PETG | Prusa: does not shrink or warp; Bambu Lab: more prone to warping than PLA | Prusa advises against one; Bambu Lab recommends an enclosed printer so a cold room does not weaken the layers |
| ABS | Prusa: significant warping; bed about 100 °C | Prusa: required, a draft shield as the fallback |
| ASA | Prusa: less than ABS, still significant | Prusa: necessary for large parts |
| PC | Prusa: warps a lot even with additives; Bambu Lab: the highest risk | Prusa: helps; Bambu Lab: a heated chamber is essential |
| Nylon (PA) | Prusa: the main drawback of pure polyamide; carbon-fibre grades warp far less | Prusa: a warm environment helps a lot |
| PP | Prusa: highly prone; brim of 5 to 10 mm | Prusa: consider one |
The makers disagree twice. Prusa says PETG barely warps, while Bambu Lab calls it more warp-prone than PLA. Prusa says carbon fibre cuts nylon's warping drastically, while Bambu Lab ranks PA-CF above plain PA.
Shape matters as much as material. Round edges warp less than sharp ones, with any filament, and more material inside the part increases warping (Prusa). Bambu Lab sees this with large prints at 60% infill, where its default is 15%, and says patterns with many straight lines shrink more than gyroid.
PLA and PETG: grip, bed heat and the first-layer fan
PLA and PETG shrink little, so a lifting corner usually means weak grip or a base that cools too fast.
Clean and match the plate. Skin oil is the number one cause of poor grip, according to Bambu Lab. Slice for the plate you use: sliced for a Cool Plate (35 °C for PLA) but printed on textured PEI (55 to 65 °C), the bed runs far too cold, and the printer skips the 0.04 mm extra squish it applies on textured PEI.
Raise the bed temperature. Add 5 to 10 °C (Bambu Lab). In a room below 20 °C, or on an open printer such as the A1, Bambu Lab adds about 10 °C more. Values per plate are in bed temperature for PLA and PETG.
Keep the fan off at the start. Bambu Lab uses no cooling for the first 3 layers for PLA, PETG and TPU: in Bambu Studio, Filament settings, Cooling, "No cooling for the first" layers. Cura's Initial Fan Speed (Cooling) starts at 0% by default. If warping continues, Bambu Lab lowers the auxiliary fan to about 40 to 50%. Prusa prints PETG's first layers with the fan off too, but for PLA with lifting corners it first checks that the print fan works, because PLA needs a lot of cooling.
Dry the PETG. Damp PETG extrudes less steadily and is more prone to poor adhesion and warping (Bambu Lab).
Do not enclose PLA like ABS. Bambu Lab opens the door or lid for PLA once the bed is above 45 °C, because a warm chamber softens the filament in the extruder; see heat creep.
Example: a flat PLA tray in a cold garage
An open-frame printer in a 16 °C garage prints a large, flat PLA tray on textured PEI at Bambu Lab's 55 °C default, and two corners lift.
Wash the plate and confirm the slicer has Textured PEI Plate selected.
The room is below 20 °C, so add about 10 °C: 65 °C, the top of Bambu Lab's 55 to 65 °C target for PLA on that plate.
Leave the first 3 layers uncooled and paint brim ears on the four corners.
Move the printer out of the draught from the door.
If the corners still lift, change the part: gyroid infill at 25% or less, and rounded corners.
ABS, ASA, PC and nylon: keep the air warm
These materials warp because the air around the print is too cold.
Enclose first. Prusa calls an enclosure required for ABS and necessary for large ASA parts. Bambu Lab closes the doors and top cover, raises the bed by 10 to 15 °C and aims for a chamber of 40 °C or more for ABS and ASA.
No enclosure: print a draft shield. A thin wall around the part keeps the air slightly warmer (Prusa). In PrusaSlicer it is Print Settings, Skirt and brim, Draft shield; in Cura, Experimental, Enable Draft Shield.
Ventilate without a draught. ABS and ASA give off fumes, so Prusa ventilates the room but keeps draughts away from the print.
Bed, speed and layout. Prusa runs ABS at 100 °C, from 80 to 110 °C depending on size, with larger parts hotter. It slows down for high-warping materials, prints several objects at once and turns the problem area towards the centre of the bed.
Enclosure and chamber details are in printing ABS and ASA. CNC Kitchen compared parts printed open and in a heated chamber; the link starts at the chapter on why chamber prints warp less.
Brim, brim ears and discs
A brim adds holding area around the base. Bambu Lab uses 8 to 10 mm for lifting PLA corners, Cura's default is 8 mm and Prusa advises at least 3 mm.
When only the corners lift, brim ears hold them and are quicker to remove. In Bambu Studio, set Brim type to Painted (Process, Others) and open the Brim Ears tool: left-click on the model adds an ear, right-click deletes one, and the automatic option places ears at corners sharper than the Maximum Angle. The ears only appear after slicing. Prusa's alternative is a tiny cylinder, a few layers tall, on the corner that lifts.
Bambu Lab's own two-minute tutorial shows brim ears being added in Bambu Studio.
Choosing between brim, mouse ears and raft, and removing them cleanly, is covered in raft, brim or skirt.
Design changes that reduce warping
If settings are not enough, change the part.
Round the corners. Round edges warp less than sharp ones (Prusa).
Split large parts. Less material means less pull; plan the seams with splitting a large model for assembly.
Break up long solid walls. Relief holes above the first layers turn one large curling force into several small ones.
Keep wide overhangs away from the bottom. Low overhangs add pulling material with little holding it down.
Use less material inside. Bambu Lab suggests about 25% infill, and no more than 50%, for strong parts.
Common mistakes
A raft under PLA. The accepted Stack Exchange answer on lifting PLA calls a raft unnecessary for PLA, and notes that a raft has no solid bottom and grips less.
Squashing the first layer harder. Prusa warns that over-squished PETG or PC can damage the PEI surface.
Changing three settings at once. Prusa and Bambu Lab lean different ways on the fan, so test one change per print.
When to change material or stop
Bambu Lab is blunt about large flat models in ABS, ASA or PC: without an enclosure they will almost always warp, so switch to PLA, PLA-CF, PETG or PETG-CF. Whether PLA or PETG can take your part's heat and load is covered in PLA or PETG for your part.
Stop and look at the hardware when the plate itself is bent, or when the printer reports a bed thermal runaway error. Prusa notes that this can happen with PC in rooms below about 18 °C, when the bed cannot hold its high temperature. Warm the room or use an enclosure, never bypass the safety check, and switch the printer off and unplug it before you work on the bed.
Next step and related guides
If a bent plate is the suspect, the build plates comparison covers flatness per plate type. If you need a large flat part rather than the practice, the 3D printing service prints PLA and PETG parts from your file; ASA only on request after a feasibility check.