Best infill pattern? Choose by what the part has to do

By Sina Esfahani, OmniTechs · Published 27 November 2026

There is no single best infill pattern, only a best pattern for each job. Infill mainly holds up the top layers from inside, and a part's strength comes mostly from its walls (Prusa). So keep your slicer's default for everyday parts, 15 to 20% grid or similar, and add walls when a part must be strong.

Change the pattern for a reason. Gyroid supports in every direction without crossing lines. Adaptive cubic saves material in large parts. Lightning and support cubic only hold up the top surface, for decorative models. Concentric suits flexible and transparent parts. On density, most models print well at 10 to 15%, and you will rarely need more than 30% (Prusa).

Choose in this order:

  1. Decorative model with no load? Lightning: the least material and time of all patterns.

  2. Everyday functional part? Keep grid, cubic or gyroid at 15 to 20%.

  3. Part that carries load? Add walls first, then raise density towards 30% for stiffness or compression.

  4. Large, bulky part? Adaptive cubic, about a quarter less material than rectilinear (Prusa).

  5. Nozzle clicking over the infill crossings? Switch from grid, triangles or cubic to a pattern without crossings, such as rectilinear or gyroid.

  6. TPU or transparent part? Concentric.

  7. Need 100%? Rectilinear; PrusaSlicer switches to it automatically.

Which pattern for which job

Infill patterns and what the makers say they are for

From the Prusa Knowledge Base, the Bambu Lab wiki fill pattern page, the OrcaSlicer wiki and Cura's base definition, read 27 November 2026. Cross Hatch and TPMS-D are in OrcaSlicer; Cross Hatch and 2D Lattice in Bambu Studio.
PatternUse it forWatch out forWho says so
GridFast general-purpose infill; good layer adhesionLines cross within a layer: material builds up, noise and nozzle strikes, worse at high speedPrusa, Bambu Lab, Cura
Rectilinear, line, zig zagSpeed and low filament use; Prusa's only choice for 100%One direction per layer, so lower strengthPrusa, Bambu Lab
Triangles, tri-hexagonEven strength in all horizontal directions and good shear resistance; tri-hexagon is among the strongest in tensionCrossing lines; top layers over triangles bridge long gapsBambu Lab
CubicFairly even strength in X, Y and Z; closed air pockets help a part float or insulateCrossing lines within a layerPrusa, Bambu Lab
Adaptive cubicLarge parts: dense near walls and top, sparse in the middleLower density in the centrePrusa, Bambu Lab
GyroidSupport in every direction with no crossing lines; can be filled with resin or liquidLonger slicing, larger G-code, vibration at high density and speedPrusa, Bambu Lab
HoneycombRigidity and impact resistanceAbout 25% more material and up to twice the print timePrusa, Bambu Lab
LightningDecorative models: builds only what the top surface needsNo strength; not for parts under loadPrusa, Bambu Lab, Cura
Support cubicHolding up top layers with little materialPrusa: no mechanical benefit; Bambu Lab's page calls it stable in X, Y and ZPrusa, Bambu Lab
ConcentricFlexible TPU parts and transparent partsWeak against sideways loads; slowPrusa, Bambu Lab
Hilbert curve, Archimedean chords, octagram spiralLooks and easy filling with liquid; chords add flexibilityLow strength; Hilbert curve is slowPrusa, Bambu Lab
Cross Hatch, TPMS-D, 2D LatticeNewer patterns: Cross Hatch for fast, non-load-bearing parts; TPMS-D strong in all directionsCross Hatch has weak points at internal corners (OrcaSlicer)Bambu Lab, OrcaSlicer

How much infill to set

Infill density and pattern the slicers ship

From the Prusa Knowledge Base and PrusaSlicer 2.9.7's profiles, Bambu Studio's shared profile and fill pattern page, OrcaSlicer's source and Cura's base definition, read 27 November 2026.
SourceDensity and patternNote
Prusa Knowledge Base10 to 15% for most modelsRarely more than 30%; 100% forces rectilinear
Prusa MK4S and CORE One 0.20 mm profiles15%, gridShipped profile in PrusaSlicer 2.9.7
Bambu Studio system profiles15%, gridOnly six patterns can print 100%
OrcaSlicer20%, Cross HatchBuilt-in default; printer profiles can change it
Cura base definition20%, gridSwitches to lines above 25%

Raise the density when the part has to be heavier, stiffer or more resistant to compression, the reasons Prusa names. Holes or bumps on a top surface can also mean too little infill underneath; that is covered in rough top surfaces, pillowing and ironing.

You set both values in one place per slicer: Process > Strength > Sparse infill density and Sparse infill pattern in Bambu Studio and OrcaSlicer, Print Settings > Infill > Fill density and Fill pattern in PrusaSlicer, and Custom settings > Infill > Infill Density and Infill Pattern in Cura. This short Bambu Lab video shows the walls, top and bottom shells and infill settings in Bambu Studio.

Episode 9: The Basic Strength Settings (Bambu Lab)

Slant 3D measured the compressive strength of a 30 mm printed cube from 10% to 100% infill, and shows how the different infills break.

From 10% to 100%: Infill Compression Strength (Slant 3D)

What each pattern costs in material and time

At the same percentage, most patterns use about the same material. Slicers space the lines to make that true: Cura places grid lines twice and cubic or triangle lines three times as far apart as single lines. The real differences are print time and the few patterns that leave volume empty on purpose.

The OrcaSlicer wiki sliced every pattern on a 100 mm cube, a 3DBenchy and the Stanford bunny at 5, 15, 30 and 50% and measured the sparse infill.

Material, print time and strength rating per pattern in OrcaSlicer's analysis

OrcaSlicer wiki, read 27 November 2026: models sliced, not printed, for a Qidi Q2 with a 0.4 mm nozzle and PLA. The wiki warns results differ per model. Strength ratings are set by hand, not tested.
PatternMaterial vs. the density setPrint time vs. baselineStrength X-Y / Z (rated by hand)
Grid0.960.77High / High
Rectilinear0.990.81Normal-Low / Low
Triangles0.970.78High / Normal
Cubic0.970.76High / High
Adaptive cubic0.580.58Normal-High / Normal-High
Support cubic0.420.47Low / Low
Lightning0.100.27Low / Low
Gyroid0.911.69High / High
TPMS-D0.981.32High / High
Cross Hatch0.931.12Normal-High / Normal-High
Honeycomb1.212.07High / High
Concentric1.361.00Low / Normal

Where the makers disagree: is gyroid fast?

Is gyroid fast? What each source says

From the Prusa Knowledge Base, the Bambu Lab wiki and the OrcaSlicer wiki's sliced estimates, read 27 November 2026.
SourceWhat it says about gyroid
Prusa Knowledge BasePrints relatively quickly
Bambu Lab wikiRelatively fast because no lines cross within a layer; longer slicing, larger G-code and strong vibration at higher density and speed
OrcaSlicer analysis, Qidi Q2 profileAbout 1.7 times the baseline time, against about 0.8 for grid

Results depend on the printer profile, so compare the time estimate on your own model.

Crossing patterns have the opposite problem. Material builds up where lines cross, and the nozzle can hit it: you hear it, at high speed it scrapes, and at worst the print fails. Grid, triangles and cubic all cross within a layer (Prusa, Bambu Lab, Cura).

Strength: direction matters more than the name

Infill strength depends on how the load arrives. A Stack Exchange answer on shear argues that patterns repeating the same path on every layer, such as grid, lines and triangles, give more bonding area between layers than 3D patterns such as cubic and gyroid; the answerer's upright gyroid bolts snapped more easily. Another answer combines two hobby tests into a rule of thumb: gyroid for shear, cubic for compression from more than one direction, triangles for compression from above. Treat both as experience, not standards.

CNC Kitchen's video crushes printed infill samples to compare how much load each pattern takes before it gives way.

TESTING 3D printed INFILL PATTERNS for their STRENGTH (CNC Kitchen)

If the part carries a real load, extra walls, a better orientation or a design change usually do more than any pattern; how strong are 3D-printed parts explains how to decide.

Patterns for special jobs

  • Flexible parts. Concentric or Archimedean chords help a TPU part flex (Prusa). Printing TPU itself is covered in how to print TPU.

  • Transparent parts. Prusa suggests concentric. Bambu Lab suggests aligned rectilinear for infill and top and bottom fill together, at the cost of strength across the lines.

  • Filling with resin or liquid. Gyroid, Hilbert curve, Archimedean chords and octagram spiral leave connected cavities (Prusa).

  • Floating or insulating parts. Cubic leaves closed air pockets (Prusa, Bambu Lab).

  • Decorative models. Lightning builds only what the top surface needs; it came from Cura and saves even more than support cubic (Prusa).

Worked example: replacing grid when the nozzle clicks

Say a PLA storage box prints with 15% grid in OrcaSlicer, and the infill takes 2 hours of the print. The nozzle clicks over the crossings and you want a quieter pattern.

  1. Gyroid removes the crossings. On the wiki's test profile its infill time was 1.69 against 0.77 for grid, about 2.2 times as long: expect roughly 4.4 hours of infill if the ratio carries over.

  2. Rectilinear also has no crossings in a layer and took 0.81, so about 2.1 hours, but it is weaker in the rating.

  3. Decide by the job. A box that only holds screws needs no strong infill: rectilinear wins. A bracket under load needs walls first, then gyroid or grid at a lower speed.

  4. Check your own estimate after slicing: the wiki's ratios come from one printer profile.

Saving time without changing the pattern

  • Thicker infill layers. PrusaSlicer can combine infill: every 3 layers at 0.1 mm gives 0.3 mm infill, up to about 80% of the nozzle diameter. Version 2.9 also has automatic infill combination. In Cura the matching setting is Infill Layer Thickness.

  • Denser only near the top. Cura's Gradual Infill Steps halve the density for each step further below a top surface.

  • Denser only where needed. A modifier raises density around a screw hole or clamp without filling the whole part; see slicer modifiers.

  • Slower infill when it fails. Rough, broken infill printed at 200 mm/s was a speed problem; the accepted Stack Exchange answer suggests starting near 60 mm/s on that printer.

When infill is not the answer

  • The part breaks under load: more walls or another orientation, not denser infill.

  • The top surface shows gaps: add top layers or fix the top settings before raising density.

  • Infill fails only at speed: look at print speed and acceleration.

To see how walls and infill share the load, read how strong are 3D-printed parts. To make only one region denser, such as the area around a screw, use slicer modifiers. If you need the part rather than the practice, the 3D printing service prints PLA and PETG parts from your file.